THE EFFECT OF MULTILAYER NANOCOMPOSITE TiAlSiN TiSiN TiAlN COATING ON CUTTING FORCES INFACE MILLING OF INCONEL 718 SUPERALLOY
ICAME 2016, 10 - 13 May 2016, (Full Text)
- Publication Type: Conference Paper / Full Text
- Süleyman Demirel University Affiliated: Yes